<div dir="ltr"><font size="6">On 10 Mar 2014 at 19:21, Keith Park wrote:<br> <br>> Problem with tar is that it will hold the moisture inside the rust scale and<br>> it will keep rotting inside the tar,<br> <br>Clean off as much rust as possible, then soak the remainder with <br>LPS-3. Let it dry, then apply the tar.<br> <br>Yes, tar over dry rust is almost pointless.<br> <br>*******************************<br>Jim Adney, <a href="mailto:jadney@vwtype3.ortha">jadney@vwtype3.or</a></font><a href="mailto:jadney@vwtype3.ortha"><font size="6">tha</font></a><font size="6"></font><br><font size="6"></font> <br><font size="6">thanks, </font><br><font size="6">fred simmons '70 sqbk <br><br id="FontBreak"><br></font></div>